Wholesale Dealers of Stainless Steel Tube Internal Threaded - GH3128 Superalloy alloy steel – Cepheus

GH3128 Superalloy alloy steel

  GH3128 alloy comprehensive performance is better than the similar GH3128 and GH3536 nickel-based solidamalgamation of gold. Suitable for manufacturing of long-term work under 950 ℃ of aircraft engine combustor flame tube, afterburner shell, regulation and other high temperature parts, main products are cold rolled sheet, also can supply hot rolled plate, bar, forging, wire and tube. GH3128 Superalloy Steel usually used in the following industries : Aero-engine combustor liner, afterburner casing, flaps Structure of the gas turbine combustor Turbine engine combustor components Afterburner parts GH3128 Superalloy alloy chemical composition:

Alloy

%

Ni

Cr

Mo

W

Fe

Ti

C

Mn

Si

V

Al

P

S

GH3128

Min

balance

19

7.5

7.5

0.4

0.1

0.4

Max

22

9.0

9.0

2.0

0.8

0.05

0.5

0.80

0.5

0.4,0.8

0.013

0.013

The resistivity of different temperature

θ/℃

20

100

200

300

400

500

600

700

800

ρ/(10-6Ω.m)

2.30

2.49

2.78

3.08

3.39

3.69

3.88

3.92

1.46

GH3128 alloy melting point : 1325-1370 ℃ GH3128 Nickel density : 8.90 g/cm3 GH3128 Superalloy Alloy is suitable for the manufacturing work under 950 ℃ of aeroengine combustor and reheater components, The effect of GH3128 is good. GH3128 main features: Superalloy (GH3128) American brands (American Standard ASTM) No corresponding grades, good solid solution strengthening type nickel base alloy overall performance, durable life and high, high plasticity, high creep strength and enduring good oxidation resistance and stamping, welding and other properties. Its overall performance is better than other similar GH3044 and GH3536 nickel-based solid solution alloys. GH3128 Product form and Specifications:

AlloySheet/Plate/Strip/Coil

Seamless alloy tube/Pipe

Welded alloy tube/pipe

Ring/Bar/Rod

Forged product

Fittings/Flange

GB/T14992-2005.

China Special Steel Limited is a GH3128 Nickel alloy Sheet/Plate/Strip/Coil/tube/Pipe/ Ring/Bar/Rod/Forging/Fittings/Flange professional manufacturer and supplier. If you have any information about GH3128 Nickel alloy chemical composition, Mechanical property, density,Heat treatment, melting point ,or any other service, please contact with our sales team.