Gh3007 / Gh5K / Iron-Based Superalloy

Product Description

GH5K superalloy Executive standard: GB/T-14992-2005 New grade: GH3007 GH5K superalloy chemical composition(%) C: ≤0.12 S: ≤0.04 P: ≤0.04 Cr: 20.0~35.0 Ni: base Fe: ≤8.0 Cu: 0.5~2.0 V: - Mo: - Ti: - Al: - Others: - GH3007 (GH5K) overview: GH3007 iron-based superalloy is developed from austenitic stainless steel and contains a certain amount of elements such as chromium and nickel. This product is at medium temperature (600~800ºC), with good mechanical properties at medium temperature and good hot working plasticity. The alloy composition is relatively simple and the cost is low.