INCONEL 22

By virtue of its contents of chromium, molybdenum, tungsten and controlled iron, this alloy exhibits excellent resistance to both oxidizing and reducing acid environments, as well as those containing mixed acids. It is particularly useful for resistance to pitting and crevice corrosion in acid-halide environments. Applications include the chemical processing, pollution control, flue gas desulfurization, waste incineration and pulp and paper processing industries.
STANDARD PRODUCT FORMS
Sheet, strip, plate, round bar, flat bar, forging stock, hexagon and wire.
MAJOR SPECIFICATIONS
USN N06022 ASTM B 366, B 462, B 564, B 574, B 575, B 619, B 622, B 626, B 751, B 775, B 829, B 906 ASME SB-366, SB-564, SB-574, SB-575, SB-619, SB-622, SB-626, SB-751, SB-775, SB-829, SB-906 ASME Code Cases 2226, N-621 Werkstoff Nr. 2.4602 ISO 6207, 6208, 9723, 9724 DIN 17744, 17750-17754
LIMITING CHEMICAL COMPOSITION, %
Ni........Remainder Cr......20.0 – 22.5 Mo.....12.5 – 14.5 Fe...........2.0 – 6.0 W............2.5 – 3.5 Co........... 2.5 max. C........ 0.015 max. Mn........0.50 max. V...........0.35 max. S...........0.02 max. Si..........0.08 max. P...........0.02 max.
PHYSICAL CONSTANTS AND THERMAL PROPERTIES
Density, Ib/in3 (g/cm3)............................................0.311 (8.61) Melting Range, °F (°C)..............2464 – 2529 (1351 – 1387) Specific Heat, Btu/lb•°F (J/kg•°C).......................0.091 (381) Curie Temperature, °F (°C)................................. <-320 (-196) Permeability at 200 Oersted (15.9 kA/m).................. <1.001 Coefficient of Expansion, 10-6 in/in•°F (μm/m•°C) 70-200°F (21–93°C)...................6.90 (12.42) 70-1000°F (21–538°C).............. 7.46 (13.43) 70-1800°F (21–982°C).............. 7.84 (14.11) Thermal ConductivityA, Btu•in/ft2•h•°F (W/m•°C)........91 (13.2) Electrical ResistivityA, ohm•circ mil/ft (μΩ•m).... 730.7 (1.215) Young’s ModulusA, 106 psi (GPa)............................ 30.3 (209) Shear’s ModulusA, 106 psi (GPa)............................ 11.0 (75.8) Poisson’s RatioA....................................................................... 0.30 HardnessA, HRB...........................................................................86 ARoom temperature, as aged.
TYPICAL MECHANICAL PROPERTIES
   