SUS310S
JIS-SUS310S
C(%) |
Si(%) |
Mn(%) |
P(%) |
S(%) |
Cr(%) |
Ni(%) |
≦0.08 |
≦1.5 |
≦2.0 |
≦0.045 |
≦0.03 |
24.0-26.0 |
19.0-22.0 |
Applications
- Heat-Resisting Stainless Steels
- Corrosion-Resisting Stainless Steels
Country Code
Steel Type
Relate Steel Type
Steel Type |
Country Code |
C(%) |
Si(%) |
Mn(%) |
P(%) |
S(%) |
Cr(%) |
Ni(%) |
|
AISI |
≦0.08 |
≦1.5 |
≦2.0 |
≦0.045 |
≦0.03 |
24.0-26.0 |
19.0-22.0 |
|
DIN |
≦0.15 |
≦0.35 |
≦2.0 |
≦0.045 |
≦0.03 |
24.0-26.0 |
19.0-22.0 |
|
GB |
≦0.2 |
1.5-2.5 |
≦1.5 |
≦0.035 |
≦0.03 |
24.0-27.0 |
18.0-21.0 |
|
JIS |
≦0.08 |
≦1.5 |
≦2.0 |
≦0.045 |
≦0.03 |
24.0-26.0 |
19.0-22.0 |
|
CNS |
≦0.08 |
≦1.5 |
≦2.0 |
≦0.045 |
≦0.03 |
24.0-26.0 |
19.0-22.0 |
|
GB |
≦0.08 |
≦1.0 |
≦2.0 |
≦0.035 |
≦0.03 |
21.0-26.0 |
19.0-22.0 |