GH3128 Superalloy alloy steel
GH3128 alloy comprehensive performance is better than the similar GH3128 and GH3536 nickel-based solidamalgamation of gold. Suitable for manufacturing of long-term work under 950 ℃ of aircraft engine combustor flame tube, afterburner shell, regulation and other high temperature parts, main products are cold rolled sheet, also can supply hot rolled plate, bar, forging, wire and tube.
GH3128 Superalloy Steel usually used in the following industries :
Aero-engine combustor liner, afterburner casing, flaps
Structure of the gas turbine combustor
Turbine engine combustor components
Afterburner parts
GH3128 Superalloy alloy chemical composition:
|
Alloy
|
%
|
Ni
|
Cr
|
Mo
|
W
|
Fe
|
Ti
|
C
|
Mn
|
Si
|
V
|
Al
|
P
|
S
|
|
GH3128
|
Min
|
balance
|
19
|
7.5
|
7.5
|
|
0.4
|
|
|
0.1
|
0.4
|
|
|
|
|
Max
|
22
|
9.0
|
9.0
|
2.0
|
0.8
|
0.05
|
0.5
|
0.80
|
0.5
|
0.4,0.8
|
0.013
|
0.013
|
The resistivity of different temperature
|
θ/℃
|
20
|
100
|
200
|
300
|
400
|
500
|
600
|
700
|
800
|
|
ρ/(10-6Ω.m)
|
2.30
|
2.49
|
2.78
|
3.08
|
3.39
|
3.69
|
3.88
|
3.92
|
1.46
|
GH3128 alloy melting point : 1325-1370 ℃
GH3128 Nickel density : 8.90 g/cm3
GH3128 Superalloy Alloy is suitable for the manufacturing work under 950 ℃ of aeroengine combustor and reheater components, The effect of GH3128 is good.
GH3128 main features:
Superalloy (GH3128) American brands (American Standard ASTM) No corresponding grades, good solid solution strengthening type nickel base alloy overall performance, durable life and high, high plasticity, high creep strength and enduring good oxidation resistance and stamping, welding and other properties. Its overall performance is better than other similar GH3044 and GH3536 nickel-based solid solution alloys.
GH3128 Product form and Specifications:
|
AlloySheet/Plate/Strip/Coil
|
Seamless alloy tube/Pipe
|
Welded alloy tube/pipe
|
Ring/Bar/Rod
|
Forged product
|
Fittings/Flange
|
|
GB/T14992-2005.
|
China Special Steel Limited is a
GH3128 Nickel alloy Sheet/Plate/Strip/Coil/tube/Pipe/ Ring/Bar/Rod/Forging/Fittings/Flange professional manufacturer and supplier. If you have any information about GH3128 Nickel alloy chemical composition, Mechanical property, density,Heat treatment, melting point ,or any other service, please contact with our sales team.